ATI 75 Nickel-Based Alloy

UNS N06075

The ATI 75™ alloy is a nickel-chromium alloy with controlled additions of titanium and carbon, which derives its high temperature strength essentially from solid solution strengthening. This alloy is used in applications requiring oxidation and scaling resistance combined with moderate strength at high operating temperatures.

Product Documents

Documents

Product Specifications By Form

Sheet

Composition

ElementMinimum (weight %)Maximum (weight %)Typical (weight %)
Cr18.021.0 
Ti0.200.60 
C0.080.15 
Fe 5.0 
Co 5.0 
Si 1.0 
Mn 1.0 
Cu 0.5 
NiBalance  

Density

lb/in3g/cm3
0.3028.37

Tensile Strength

ksiMPa
110 min760 min

Yield Strength

ksiMPa
45 min310 min

Elongation

30% min

Specifications

BS 2HR 203, DIN 17750, DIN 17742, ISO 9722, ISO 6208